POLYCRYSTALLINE SHARPENING (PDC)
| COMPOSITION |
|
|
| 75W-25Cu |
|
|
| |
|
|
| DENSITY gr/cm3 |
Conduc% Iacs |
Brinnel hardness |
| 14,85-15,05 |
46-50 |
200-210 |
PERIPHERAL 1A1 SHAPE
| DIAMETER |